    Have looked at Pewter previously but sort of scrubbed it due to the antimony and copper content, but at 20:1 lead to tin then they would end up as very small % in the final mix.

    I’m reluctant to change from something that works I suppose?

    T

  2. #2
    Join Date
    May 2009
    Location
    Reading
    Posts
    4,806
    Quote Originally Posted by thibben View Post
    Kenny

    Have looked at Pewter previously but sort of scrubbed it due to the antimony and copper content, but at 20:1 lead to tin then they would end up as very small % in the final mix.

    I’m reluctant to change from something that works I suppose?

    T
    not a problem just throwing it out there
    You Cannot Reason People Out of Something They Were Not Reasoned Into
    "Politicians like to panic, they need activity. It is their substitute for achievement" Sir Humphry Appleby

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •